Chemical Name: Poly-tert-Butylphenoldisulfide
CAS No.:60303-68-6
Molecular formula:(C10H14O)x▪(Cl2S2)y
Appearance:Yellow to reddish granules
Sulfur content,%:29.5-31.5
Softening Point,℃:95-115
TB7 is the sulfur donor for natural and synthetic rubbers. Itproduces ahigh percentage of mono-sulfidic crosslinks that results in vulcanizates with superior aging characteristics.Itcan be used as either complete or partial replacements for sulfur and thiuram and DTDM sulfur donors in EV and semi-EV type cure systems. In tires TB7 serials are used in the innerliner, chafer, bead apex, sidewalls, and tread.
Polymers: Natural rubber and synthetic elastomers. Especially good in curing rubber that contains chlorine such as chlorobutyl and polychloroprene.
Synergism:It can be used with most typical rubber accelerators and sulfur. Whenit isused as a partial
replacement for sulfur, TB7 tends to improve dispersion of other additives in the rubber.
Crosslink Type: TB7 promotes mono-sulfidic crosslinks resulting in vulcanizates with excellent heat and aging resistance.
Non-nitrosamine: TB7 does not produce nitrosamines like many of the other sulfur donors such as DTDM and the thiurams. info at hhochem. com