Main Features:
1. High expansive performance: 7d between the water limit expansive ratio can reach 0.15 - 0.2%. It is 4 - 8 times the expansive volume of ordinary expansive agent.
2. Expansive rate is proper: the 3d water limit volume of expansion can be up to 70 - 80%, 7d was above 85%.
3. Under the condition of 100% dry, it can still maintain larger expansive volume.
4. The performance is stable.
Technical data:
Index | Type 100 | Type 130 | Type 160 | |
Fineness | Specific surface area (m2/kg) ≥ | 200 | ||
1.18mm residue on sieve (%) ≤ | 0.5 | |||
Setting time (min) |
Initial setting time (min) ≥ | 45 | ||
Final setting time (min) ≤ | 600 | |||
Limit expansive ratio (%) | In the water 7day ≥ | 0.100 | 0.130 | 0.160 |
In the air 21day ≥ | -0.020 | -0.010 | -0.010 | |
Compressive strength (MPa) | 7day ≥ | 20 | 20 | 20 |
28day ≥ | 40 | 38 | 35 | |
Remarks: the limit expansive ratio in the table is |
Application:
1. Make all kinds of high-grade special mortar and
Main Features: 1. High expansive performance: 7d between the water limit expansive ratio can reach 0.15 - 0.2%. It is 4 - 8 times the expansive volume of ordinary expansive agent. 2. Expansive rate is proper: the 3d water limit volume of expansion can be up to 70 - 80%, 7d was ...
mould release agent for concrete products use for Steam Curing Auto Control System for Precast Concrete Segment of Shield ...