Item(HP) | (mm) | 200-400 | 450-500 | |
Electrical Resistivity | E | μΩ-m | ≤7.0 | ≤7.5 |
N | ≤6.5 | ≤6.5 | ||
Breaking Strength | E | MPa | ≥10.5 | ≥9.8 |
N | ≥14.0 | ≥14.0 | ||
Elastic Modulus | E | GPa | ≤12.0 | ≤12.0 |
N | ≤16.0 | ≤16.0 | ||
Density | E | g/cm³ | ≥1.65 | ≥1.60 |
N | ≥1.72 | ≥1.70 | ||
CTE | E | 10-6/°C | ≤2.4 | ≤2.4 |
N | ≤2.2 | ≤2.2 | ||
Ash | % | ≤0.3 | ≤0.3 |