* Low shrinkage (less than 0.1% )
* High tensile and tear strength with high copy times
* Hing heat resistance which can up to 250 °C
* Easy for operation (mixing ratio at 1:1 /10:1)
* Very good flow and easy for pouring operation
* Fast and non-shrink cure at room temperature which can be accelerated considerably by the application of heat