NON ASBESTOS JOINTING SHEETS


 

  6.          IGNITION LOSS                 DIN 52911                     %                  ? 30

                INCREASE IN MASS                                            %                   ?15
                INCREASE IN THICKNESS                                   %                   ?  5

       (c) IN WATER/ANTIFREEZE    ASTM F 146

                INCREASE IN MASS                                            %                   ?10
                INCREASE IN THICKNESS                                   %                   ?  7

(b) IN FUEL B                        ASTM F 146

                 INCREASE IN MASS                                            %                   ?10
                 INCREASE IN THICKNESS                                   %                   ?  8

(a) IN ASTM OIL NO. 3           ASTM F 146            

  5.           FLUID ABSORPTION        

  4.           RECOVERY                        ASTM F36A                 %                  ? 50

  3.           COMPRESSIBILITY            ASTM F36A                 %                  6 12

  2.          TENSILE STRENGTH  
               (a) ACC to ASTM F152(ACROSS GRAIN)                N/MM2               14  Min.  
               (b) ACC to DIN52910    (ACROSS GRAIN)               N/MM2                11 Min.

THICKNESS                    : 0.25 mm to 3.00 mm.
OPERATING CONDITION : Maximum Peak Temp.    : 400
  • Country:India
  • telephone:91-911202700291
MATERIAL GRADE : FEROLITE NAM 32
*Your name:
*Your Email:
*To:Ferolite Jointings Limited
*Subject:
*Message:
Enter between 20 to 3,000 characters. English only.     Characters Remaining: 0 / 3000
*Enter the secure code shown below Mfrbee security Image      Reload Image

We do inquire for you , please wait ...