6. IGNITION LOSS DIN 52911 % ? 30
INCREASE IN
MASS
% ?15
INCREASE IN
THICKNESS
% ? 5
(c) IN WATER/ANTIFREEZE ASTM F 146
INCREASE IN
MASS
% ?10
INCREASE IN
THICKNESS
% ? 7
(b) IN FUEL B ASTM F 146
INCREASE IN
MASS
% <=10
INCREASE IN
THICKNESS
% ? 8
(a) IN ASTM OIL NO. 3 ASTM F 146
5. FLUID ABSORPTION
4. RECOVERY ASTM F36A % ? 50
3. COMPRESSIBILITY ASTM F36A % 6 - 12
2. TENSILE STRENGTH
(a) ACC to ASTM F152(ACROSS
GRAIN)
N/MM2 >=14
(b) ACC to DIN52910 (ACROSS
GRAIN)
N/MM2 11
|
MATERIAL GRADE : FEROLITE NAM 32 STEEL |