(1) Drill hole
(2) Insert anchor.Expand by hammer.
(3) Tighten the steel wire or rod.
Production range:Diameter. 6mm-20mm Length:25mm-150mm
the test pulling force value listed beneath were obtained using 200-250kgs/cm 2 concrete (no aggregated)
pressembled for quick and easy installation
Applicable parent metal: concrete and thick natural stone.
Application: fire dydrant,installation of hot-water pipe air-conditioner and exhaust duct,panel wall,
Matrial:commen carbon steel,stainless steel
(1) Drill hole
(2) Insert anchor.Expand by hammer.
(3) Tighten the steel wire or rod.