Lamineries MATTHEY further offer a broad assortmentof stainless austenitic steel, supplied in form of thin precision foilsand strips, with a thickness of less than 0.010 mm
The mechanical strength of austenitic stainlesssteel is normally average, may however be increased substantially bycold rolling in case of certain types. A higher mechanical strength isobtained with steel 1.4310, X10CrNi18-8, its austenitic structure ishowever unstable and corrosion resistance is lower compared to 1.4435,316L. A higher mechanical strength of steel 1.4310, X10CrNi18-,typically at 80 to 250 N/mm2 (depending on hardness grade)is achieved by annealing at a temperature between 380 and 420
Lamineries MATTHEY produces a broad assortment of stainless austenitic steel, supplied in form of thin precision strip and foil.
Steel Grade: | 300 Series |
Certification: | Other |
Technique: | Cold Rolled |
Place of Origin: | Switzerland |
Width: | 0.5-200 mm |
Thickness: | 0.003-1.0 mm |
Standard: | Other |