type
oz/ft coating
designation
previous
coating class
(of sheet) oz/ft
(of sheet)
Alloyed A 60
A 40
A 25
A 01 -
-
-
- 0.60
0.40
0.25
No Minimum 0.50
0.30
0.20
No Minimum
minimum check limit
triple-spot testing single-spot testing
astm a525
This sheet steel is heat treated after coating to produce a zinc-iron alloy and eliminate the spangle. Even though the zinc alloy lacks ductility and with severely formed parts, powdering of the surface sometimes occurs in localized areas, only the zinc coating comes off and a protective alloy bond remains. It will withstand temperatures in the range of 750
This sheet steel is heat treated after coating to produce a zinc-iron alloy and eliminate the spangle